Faulty Sakno siliconefoamfirestop installation in a Calgarywastewater treatment plant in the 1980's. This is a hole in a fire-resistance ratedconcrete wall, above a fire door frame. The outside temperature was ca. -40°C (-40 F). The inside was heated. A steady temperature is needed for the foam to "snap", solidify and expand properly, as it evolves hydrogengas. Every now and then someone opened the outside door, the temperature would plummet and the foam's consistency was affected, as can be seen by the tears and uneven bubble distribution and incomplete phase change. To achieve its rating, as per its certification listing, the foam also requires ceramic fibre boards (furnace insulation) to permanently cover both sides of the foam, a common deficiency, exposed by whistleblower Gerald W. Brown. This is image 1 of 2. The other one is right here: http://commons.wikimedia.org/wiki/Image:Silicone_foam_sakno2.jpg .
Cette œuvre a été placée dans le domaine public par son auteur, I, Achim Hering. Ceci s’applique dans le monde entier. Dans certains pays, ceci peut ne pas être possible ; dans ce cas : I, Achim Hering accorde à toute personne le droit d’utiliser cette œuvre dans n’importe quel but, sans aucune condition, sauf celles requises par la loi.
Cette image (ou toutes les images dans cette catégorie/page) est irrémédiablement floue, ou trop claire, ou trop foncée, ou ne montre pas suffisamment bien le sujet qu'elle est censée illustrer. S'il existe une image de meilleure qualité, pensez à remplacer celle-ci avec. Sinon, essayez de vous procurer une image de remplacement (sous licence libre) sur Internet.